Product Name Robot Laser Welding Machine
Laser Power   1500W 2000W 3000W 6000W optional
Laser Source Raycus IPG JPT MAX BWT optional
Robot Arm TAIYI Yaskawa ABB KUKA
Laser Wavelength 1070nm
Pulse Width 0-5ms
Pulse Frequency ≤100Hz
Spot adjusting range 0.1-3mm
Repeating precision ±0.01mm
Cooling System Water Cooling
Robot arm length 143cm/150cm/173cm/200cm/220cm

05.jpg06.jpg07.jpg08.jpg09.jpg

1.Automotive Industry

Body-in-White (BIW)Manufacturing:Laser welding  for door  frames,roof seams,and chassis components,ensuring lightweight and high-strength joints.

Battery Production:Welding lithium-ion battery cells,busbars,and  connectors for EVs(e.g.,Tesla’s  battery packs).

Powertrain  Systems:Precision welding of transmission components  and  engine  parts. Advantages:Reduced thermal distortion,high repeatability,and  compatibility with

advanced materials (aluminum,high-strength  steel).

2.Electronics  &Semiconductor  Manufacturing

Microelectronics:Hermetic sealing of sensors,microcircuits,and  MEMS devices.

Consumer Electronics:Welding smartphone casings(e.g.,aluminum alloy  frames)and 

battery tabs.

PCB Assembly:Joining fine connectors and shielding components.

Advantages:Minimal heat-affected  zone(HAZ),suitable for heat-sensitive components.

3.Medical Device Industry

Surgical Instruments:Welding stainless steel  scalpels,forceps,and  endoscope parts. Implantable Devices:Sealing pacemakers,orthopedic implants,and dental prosthetics.

Diagnostic  Equipment:Assembly of  MRI/X-ray machine  components.

Advantages:High hygiene  standards,precision for miniaturized parts,and biocompatible welds

4.Aerospace &Defense

Aircraft Structures:Welding turbine blades,fuel nozzles,and fuselage panels(e.g.,titanium alloys).

Satellite Components:Joining lightweight  materials (e.g.,aluminum-lithium al loys) for space applications.

Military Hardware:Armor plating and missile guidance system assembly.

Advantages:Deep-penetration welding,compatibility with refractory metals, and compliance with strict aerospace standards.

11.jpg

10

Reviews

There are no reviews yet.

Be the first to review “Robotic Laser Welding Machine with Long-Life Laser Source 1500W-3000W Durable”

Your email address will not be published. Required fields are marked *